Steel Aluminum
| Question | Answer |
|---|---|
| Stainless Steel gasses | Argon and Helium |
| 400 series stainless steel benefit is ___________________ | prevents corrosion at high heat |
| Purging gasses for Stainless | Argon, Helium, Nitrogen |
| Chromium does what? | creates a protective shield on stainless, it prevents corrosion at high heats |
| How much Chromium (Cr) is needed to be Stainless Steel | at least 10% |
| Austenitic stainless steel is___________________ | not magnetic, has the highest corrosion resistance and is the most ductile |
| 500 series steel | is not stainless steel |
| Sugaring is caused by? | Oxidation from lack of shielding gas |
| Back gas should be used on what materials? | alloy steel, stainless steel, aluminum and copper |
| Gas used for aluminum welding? | Helium and Argon |
| What is the beginning of material of aluminum | Bauxite |
| How much more distortion from heat does stainless steel have over mild steel? | 50% more |
| Which series of stainless steel does not need a pre-heat? | 300 series |
| Aluminum GMAW is used in ____________________ polarity | DCEP |
| Most common filler metal for Aluminum | ER 4043 |
| Aluminum GMAW drive rolls are _________________ | U-groove |
| Aluminum GTAW polarity is _________________ | High Frequency alternating Current (AC) |
| What is the maximum safe preheat temperature for Aluminum? | 66 degrees Celsius |